PP-AN163

Flux-cored wire for automatic and semi-automatic open-arc, submerged-arc or gas-shielded hardfacing of parts exposed to cyclic loads, corrosion, cavitation erosion, and metal-to-metal friction.

Order form 
Additional Information
Diameter, mm 1.6 - 4.0
Curent type / Shielding DC+ / Open arc, Flux, Ar, Ar + CO2
Working conditions Cyclic loads, corrosion, cavitation erosion, and metal-to-metal friction.
Applications

Hardfacing of marine shaft collars, stocks, rudder spindles, steel crankshafts, parts of drilling, pilger mill rolls, etc.

 
Recommended flux  EFA-1, АN-26S/P, АN-20S/P
Slag separation good
Deposit factor, g/A·h 14 - 18
Crack susceptibility low
Wire consumption, kg 1.05 - 1.2
Hardness of weld metal HRC 33 - 40

OPERATING CONDITIONS (submerged arc)

Wire diameter, mm

Current, A

Voltage, V

Deposition rate, m/h

1.6

150 – 230

27 – 30

8 – 15

2.0

180 – 280

29 – 31

10 – 18

2.4

220 – 320

30 – 32

13 – 20

2.8

260 – 380

31 – 33

14 – 22

3.2

300 – 430

32 – 34

15 – 25

Similar products
Flux-cored wire for automatic and semi-automatic submerged-arc hardfacing of parts exposed to metal-to-metal friction, cyclic thermal load and high relative pressure.
Flux-cored wire for automatic and semi-automatic open-arc or submerged-arc hardfacing of parts exposed to cyclic loads, corrosion, cavitation erosion, and metal-to-metal friction.
Flux-cored wire for submerged-arc hardfacing of parts exposed to thermal fatigue and substantial relative pressure.
Flux-cored wire for automatic and semi-automatic submerged-arc or gas-shielded hardfacing of carbon steel parts exposed to metal-to-metal friction and abrasive wear.
Flux-cored wire for submerged-arc or gas-shielded hardfacing of parts exposed to thermal fatigue and high relative pressure.
Flux-cored wire for automatic and semi-automatic submerged-arc hardfacing of steel mill rolls exposed to metal-to-metal friction, cyclic thermal load and corrosion.